Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /home3/weldingw/public_html/wp-includes/functions.php on line 6114

Notice: session_start(): Ignoring session_start() because a session is already active in /home3/weldingw/public_html/wp-content/themes/responsive-child/header.php on line 3
Nickel 903 - The Welding Warehouse, Inc. Nickel 903 - The Welding Warehouse, Inc.

Nickel 903

GTAW Solid Bare Welding Wire, Iron Base — Nickel 903


Nickel 903

Nickel 903 is a low expansion, high temperature, high strength nickel-cobalt-iron filler metal used to produce high quality welds in matching base metals. Large amounts have been used for space shuttle rockets and similar vessels.

Applications:

Stringer beads with controlled low heat input and ultra clean weldment conditions are essential for sound welds.


Specifications:

  • UNS N19903
  • AMS 5806
  • USWC 5806 (V)
  • Incoloy 903
  • 42Fe 38Ni 15Co 3Cb+Ta 1.4Ti 0.92Al (VM)
Nominal Chemical Composition (%)
C Mn Si S P Cr Ni Mo Co
0.06 max 1.00 max 0.35 max 0.008 max 0.015 max 1.00 max 36.00-40.00 0.20 max 13.00-17.00
Nb Ti Al B Cu Ca O N Fe
2.40-3.50 1.20-1.60 0.70-1.15 0.003 max 0.20 max 0.0010 max 0.0025 max 0.0050 max Bal
Typical Weld Properties
Density Melting Range
8.25gm/cc 2400°-2540°F