Magnesium AZ91A
AZ91A
AZ91A, B, C, D, and E have the same nominal composition but differ in ranges and/or specified impurity limits. The die cast alloy in as-cast condition (F) can be made for secondary metal, reducing the cost of the alloy. Must be used when maximum corrosion resistance is not required.
Specifications:
- UNS M11910
- AMS 4490
- ASTM B 94
- SAE J465
- European EN 1753
- MC 21120
Typical Chemical Composition (%) | ||||||
---|---|---|---|---|---|---|
Al | Cu | Mg | Mn | Ni | Si | Zn |
8.3-9.7 | ≤0.10 | 90.0 | ≥0.13 | ≤0.030 | ≤0.50 | 0.35-1.0 |