E409T
E409T is a flux cored, electrode with a nominal composition of 12% chromium, with titanium added as a stabilizer to produce a ferritic microstructure.
Specifications
- E409T0-0
- E409T0-1
- E409T1-1
- E409T1-4
- E409TX-X
Welding Positions
Flat and Horizontal (0-X)
All Position (1-X)
Typical Chemical Composition |
C |
Mn |
Si |
Cr |
Ni |
Mo |
P |
S |
Ti |
Cu |
0.10 max |
0.80 max |
1.00 max |
10.5-13.5 |
0.60 max |
0.50 max |
0.04 max |
0.03 max |
10xC min – 1.5 max |
0.50 max |
Typical Mechanical Properties |
Tensile Strength |
65,000psi min |
Elongation |
15% |