AWS 5.14 ERNiCrFe-6
INCONEL® Filler Metal 92
INCONEL® Filler Metal 92 is used for gas-tungsten-arc and gas-metal-arc welding of austenitic and ferritic steels and nickel alloys. Applications include joining INCONEL® and INCOLOY® alloys to stainless steels, carbon steels, and MONEL® alloys; joining MONEL® alloys metal is also used for welding nickel steels. The high Ti concentration provides excellent porosity resistance in field welding applications.
INCONEL® Filler Metal 92 provides high strength and corrosion resistance at temperatures ranging from the cryogenic region to over 1800°F (980°C). Weld deposits can be age hardened for greater strength at temperatures to about 1300°F (700°C)
Specifications:
- AWS A5.14 ERNiCrFe-6 (UNS N07092)
- ASME II, Part C, SFA-5.14, ERNiCrFe-6 (UNS N07092)
- ASME IX, F-No.43
- BS 2901 NA39
- (EN) ISO 18274-SNi 7092 (NiCr15Ti3Mn)
For manufacture to ASME III (NCA3800, NB2400), MIL, Rolls Royce, AMS and other specifications please refer your inquiry to the Technical Department prior to order placement.
| Nominal Chemical Composition (%) | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Ni+Co | C | Mn | Fe | S | Si | Cu | Cr | Ti | P | Others |
| 67.0 min | 0.08 max | 2.0 2.7 | 8.0 max | 0.015 max | 0.35 max | 0.50 max | 14.0-17.0 | 2.5-3.5 | 0.03 max | 0.50 max |
| Minimum Mechanical Properties (As Welded) | |
|---|---|
| Tensile Strength (psi) | 94,000 |
| Tensile Strength (MPA) | 648 |
| Elongation (4d) % | 42 |