AWS A5.13 ECoCr-B


Cobalt 12

ECoCr-B electrodes and rods are similar in composition to deposits made using ECoCr-A (Cobalt 6) electrodes and rods, except for a slightly higher percentage (approximately 16%) of carbides. The alloy also has a slightly higher hardness and better abrasive and metal-to-metal wear resistance. Impact and corrosion resistance are lowered slightly. Deposits can be machined with carbide tools.

ECoCr-B (Cobalt 12) electrodes are used interchangeably with ECoCr-A (Cobalt 6) electrodes. Choice will depend on specific application.


Nominal Chemistry Composition (%)
C Mn Si Cr Ni Mo Fe W Co OE
1.0-1.7 1.0 max 2.0 max 25-32 3.0 max 1.0 max 5.0 max 7.0-9.5 BAL 1.0 max
Minimum Mechanical Properties
Hardness (HRC) 34-47