AWS 5.14 ERNiFeCr-2
INCONEL® Filler Metal 718
INCONEL® Filler Metal 718 is used for gas-tungsten-arc welding of INCONEL® alloys 718, 706 and X-750. The weld metal is age hardenable and has mechanical properties comparable to those of the base metals.
The filler metal can be used with both the gas metal arc and gas tungsten arc processes.
Specifications:
- AWS A5.14 ERNiFeCr-2 (UNS N07718)
- ASME II, Part C, SFA-5.14, ERNiFeCr-2 (UNS N07718)
- BS2901 NA 51
- DIN 1736 SG-NiCr19NbMoTi (2.4667)
- (EN) ISO 18274 – SNi7718 (NiFe19Cr19Nb5Mo3)
For manufacture to ASME III (NCA3800, NB2400), Rolls Royce, AMS and other specifications please refer your inquiry to the Technical Department prior to order placement.
Nominal Chemical Composition (%) | ||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Ni | C | Mn | Fe | S | Si | Cu | Cr | Al | Ti | Nb+Ta | Mo | P | B | Co |
50.0-55.0 | 0.08 max | 0.35 max | Remainder | 0.015 max | 0.35 max | 0.30 max | 17.0 to 21.0 | 0.20-0.80 | 0.65-1.15 | 4.75-5.50 | 2.80-3.30 | 0.015 max | 0.006 max | 1.0 max |
Minimum Mechanical Properties | |
---|---|
Tensile Strength (psi) | 165,000 |
Tensile Strength (MPA) | 1138 |
(Age hardened condition: 1325°F (720°C)/8 hours, Furnace Cool 100°F (55°C)/hour to 1150°F(620°C)/8 hours, Air Cool)