ER2509
Alloy 2509 is a bare, corrosion resistant, super duplex rod for welding austenitic-ferritic stainless alloys of the 25% Cr, 7% Ni, 4% Mo, low C type. Alloy 2509 has high intergranular corrosion, pitting and stress corrosion resistance. The alloy is widely used in applications where corrosion resistance is of the utmost importance, such as the pulp & paper, offshore and gas industries.
Specifications
Nominal Chemical Composition (%) |
C |
Si |
Mn |
Cr |
Ni |
Mo |
W |
Cu |
<0.02 |
0.4 |
0.4 |
25.0 |
9.8 |
4.0 |
<1.0 |
<0.3 |
Typical Mechanical Proprerties |
Tensile Strength |
Yield Strength |
Elongation |
670 MPa |
850 MPa |
30% |
Charpy V |
Test Temps °C |
Impact Values J |
+20 |
150 |
-40 |
115 |